06-09-2015, 02:14 AM
I bought and used the Stabond on my Fuzion (because of the rough texture of the boat) I did the three coat thing. It is holding well after a year but the D rings are coming up a little.
On the smooth material of the Outcast, you can probably use the single coat stabond (make sure for Vinyl).
My boats are more a Urethane cover (except the Predator) I used the two part Sta Bond on three of my boats. On the other two I used LOC TITE for Vinyl. It is about one third the cost, last longer and seems to hold up as well after three years so far.
Good luck.
[signature]
On the smooth material of the Outcast, you can probably use the single coat stabond (make sure for Vinyl).
My boats are more a Urethane cover (except the Predator) I used the two part Sta Bond on three of my boats. On the other two I used LOC TITE for Vinyl. It is about one third the cost, last longer and seems to hold up as well after three years so far.