06-09-2015, 01:33 PM
I also did the 3 coats while Ive never used Stabond if its anything like Vyna-bond the glue and glue process is a little different than normal glue or what im use too.
You wipe on the glue and wait for about 5 minutes the glue needs to set or be partially dried and tacky. By putting on a second or 3rd coat you reactivate the glue and add another layer or more glue for adhesion.
For rod holders 1 to 2 layers probably would suffice but in the NRS video they use 3 layers for D-rings and Foot cups due to the increased pressure these attachments will get.
Oh and on a side note ( FG taught me this) get you a Big bottle of 303 aerospace protectant and wipe down your toon down every so often it will keep the sun from fading the color from your toon.
[signature]
You wipe on the glue and wait for about 5 minutes the glue needs to set or be partially dried and tacky. By putting on a second or 3rd coat you reactivate the glue and add another layer or more glue for adhesion.
For rod holders 1 to 2 layers probably would suffice but in the NRS video they use 3 layers for D-rings and Foot cups due to the increased pressure these attachments will get.
Oh and on a side note ( FG taught me this) get you a Big bottle of 303 aerospace protectant and wipe down your toon down every so often it will keep the sun from fading the color from your toon.
[signature]